Welding Wires
The carbon steel & low alloy steel gas shield flux-cored wire
The welding wire for titanium type slag system CO2 gas shielded flux-cored wire. Be applicable to set down welding in all positi
1. The carbon steel and the low alloy steel flux-cored wire StyleChinese standardU.S.A.(AWS)JapanDia(φmm)tensile strength(Mpa)yield...
Stainless steel submerged arc welding wire
Stainless steel flux-cored wire in the application of MAG welding primarily. high efficiency deposition rate,easy to slag off.
GradeWith fluxEqual tochemical composition(%)tensile...
Gas shielded welding wire
Apply to the carbon steel and the low alloy steel 500 MPa level of single channel and multi-channel welding
StyleChinese standardU.S.A(AWS)Japan(JIS)tensile strength(Mpa)yield strength(Mpa)elongation(%)Akvballisticwork(J)room temperatureshielding gasMelt the deposited metal main...
TH-E71T-1 Low carbon steel gas shielded flux-cored welding wire
Including made downward welding in all position welding. Weld spatter is small, arc stability downy. Deslagging easy, weld appea
Deposited metal chemical composition ( Protective gas: CO2 ) (%) CMnSiSP≤0.12≤1.75≤0.90≤0.030≤0.030 Deposited metal...
Heat resistant steel flux-cored welding wire
The dc reverse connect, can all position of welding
StyleChinese StandardU.S.A(AWS)Dia(φmm)tensile strength(Mpa)yield strength(Mpa)elongation(%)Akvballisticwork(normal temperature)Melt the deposited metal main chemical composition(%)Main UsageCMnSiSPTH-R302E551T1-B2 1.2 /...
Submerged Arc Welding Wire
for carbon steel and low alloy steel structure,such as Bridge,boilers
chemical composition(%)GradestandardStandardCMnSiCrNiSPCuTH-H08AH08AAWS EL-8JIS W11≤0.100.30-0.60≤0.03≤0.20≤0.30≤0.0300.030≤0.20TH-H08MnAH08MnAAWS EM-12JIS...
Stainless steel argon arc welding wire
General need not preheating, need 150 degree above the preheating. 250-300 degree under 30 to 60 minutes to dry.
GradeEqual tochemical composition(%)tensile strength(MPa)elongation(%)usageAWSGBCMnSiCrNiothersTH-ER308ER308H0Cr21Ni100.051.790.3319.7210.14-5804218%Cr-8%Ni stainless...